Crash Machine
100 W
The Fusin battery still works. It's a well constructed battery with a key switch and a fuse inside a steel box. I have over a thousand miles on it. The problem is major voltage sag. It's not uncommon to see it sag below 48v until it finally cuts out at 44v. Any hill above 6% has me switching down to med. speed with the three speed switch. Any steeper and I'm down to low speed and peddling. I've been noticing a drop in amp hours till finally the other day at 7.1 amp hours it left me peddling home. Hot off the charger it reads 53.4v. But it doesn't take long to settle at 50v when under use. The Ping doesn't have this problem at all. Is it as simple as a not enough c rating?. When I tested the individual cells they were all the same. My voltmeter is messed up so I can't give exact numbers till it's fixed. Here's a pic. of it. I have the battrey out of the case and will post pics. of that this evening. Thank you for everyones input about the diodes. I was going to open another thread about this battery but since you asked...