DrInnovation
⚡ Regular
Hi.. looking on advice for dealing with my Lashout ebike (synergy/rayous parent, Currie cousin). It has a 600w MAC motor with integrated controller and a plantary gearing system that drives the #25 chain that is attached on the disk mounting.
Bougth it used.. had a problem when the bolts fell off and the motor came loose -- motor was hanging by its wires. I think some dirt got in, so I cleaned out the gears (wd40) and then I repacked it with lithium grease. Been working smoothly but yesterday it was working the battery super hard (though maybe I lost a pack in series). and when I got home it would not backup at all and would not freewheel properly either.
So I took it appart and the grease was silver from the number of metal particles in it. Given the volume of metal i knew it was serious so I totally disassbled the planetary. No missing teeth but the plate that holds the gears was highly worn.. look at the sections point to by the red arrow and you can see the missing metal worn off the alignment posts.


You can also see the wearing it did on the motor face

Cleaned it up and reassembled and repacked it with grease..

but now its making a horrible noise when under load.. you can hear it in the following movies.
View attachment Lashout-Grind.mp4
Is it possible I repacked something wrong which lead to the grinding? Any ideas how to fix it?So.. Is the existing planetary gear just toast? Is it something else?
There is a fair amount of play in the sprock (in and out).. could that mean I lost something else (a spacer or something?).
I'm heavy (235lb with pack) and taking this up steep hills (8%, 10%).. the hills are too steep for the bike on its own.. I have to pedal). Is that just too much stress for this old unit..
If I buy a replacement planetary is it likely it will die the same type of death (I've been riding 5x a week since june..
Bougth it used.. had a problem when the bolts fell off and the motor came loose -- motor was hanging by its wires. I think some dirt got in, so I cleaned out the gears (wd40) and then I repacked it with lithium grease. Been working smoothly but yesterday it was working the battery super hard (though maybe I lost a pack in series). and when I got home it would not backup at all and would not freewheel properly either.
So I took it appart and the grease was silver from the number of metal particles in it. Given the volume of metal i knew it was serious so I totally disassbled the planetary. No missing teeth but the plate that holds the gears was highly worn.. look at the sections point to by the red arrow and you can see the missing metal worn off the alignment posts.


You can also see the wearing it did on the motor face

Cleaned it up and reassembled and repacked it with grease..

but now its making a horrible noise when under load.. you can hear it in the following movies.
View attachment Lashout-Grind.mp4
Is it possible I repacked something wrong which lead to the grinding? Any ideas how to fix it?So.. Is the existing planetary gear just toast? Is it something else?
There is a fair amount of play in the sprock (in and out).. could that mean I lost something else (a spacer or something?).
I'm heavy (235lb with pack) and taking this up steep hills (8%, 10%).. the hills are too steep for the bike on its own.. I have to pedal). Is that just too much stress for this old unit..
If I buy a replacement planetary is it likely it will die the same type of death (I've been riding 5x a week since june..