Samsung 35E vs 30Q Cycle Life

In short yes, MJ1 is the king of the cycle life at low loads up to 1C average discharge. LG MJ1 holds >85% of its initial capacity after 1000 cycles at 100% DoD cycling 0.5C charge - 1C discharge.
 
Pajda said:
In short yes, MJ1 is the king of the cycle life at low loads up to 1C average discharge. LG MJ1 holds >85% of its initial capacity after 1000 cycles at 100% DoD cycling 0.5C charge - 1C discharge.
Thanks - that's what I am gathering from the info I can gather. Also the LG M36 looks very similar. It's a bit cheaper from Queen battery. Would you expect it to be equally as good?
 
Back
Top