townunheardof
1 mW
Hey,
After 3.5 years with my SLAs on my Wilderness Energy 36v brushless, my 48v 15ah LifePo4s arrived from Hong Kong a week ago and I got them charged yesterday and mounted today.
First impressions: Nicely made, better presentation than I expected, solid pack, duct taping even done neatly and as professional as gray duct tape can be. And at about $450 all in, I'm happy with the price.
Coupla questions:
I haven't been able to find anything clear on this searching the history here....do Lifepo4s need breaking in?
I charged with the 5.0 amp charger all day yesterday, about 10 hours.
This morning I mounted the pack and took a ride. I liked the performance. Seems to have a different power curve than my SLAs, though they are 2.5 years and about 400 charge cycles old. Smoother, a bit faster, more power, but not strikingly more.
Then, about 5 miles into the ride (fortunately I was 1/2 mile from home) power went to virtually nothing. Its like the pack just ran down to nothing.
Is there a break-in period with this chemistry? Do I need to do some shallow charge cycles or something?
I switched to Lifepo4 for greater range and power. 5 miles ain't gonna cut it.
Maybe I didn't charge long enough? Should the first charge time be longer than 10 hours?
Also: Another topic, mechanical: I saw something in here about a Torque Arm. Do I need one?
Town
After 3.5 years with my SLAs on my Wilderness Energy 36v brushless, my 48v 15ah LifePo4s arrived from Hong Kong a week ago and I got them charged yesterday and mounted today.
First impressions: Nicely made, better presentation than I expected, solid pack, duct taping even done neatly and as professional as gray duct tape can be. And at about $450 all in, I'm happy with the price.
Coupla questions:
I haven't been able to find anything clear on this searching the history here....do Lifepo4s need breaking in?
I charged with the 5.0 amp charger all day yesterday, about 10 hours.
This morning I mounted the pack and took a ride. I liked the performance. Seems to have a different power curve than my SLAs, though they are 2.5 years and about 400 charge cycles old. Smoother, a bit faster, more power, but not strikingly more.
Then, about 5 miles into the ride (fortunately I was 1/2 mile from home) power went to virtually nothing. Its like the pack just ran down to nothing.
Is there a break-in period with this chemistry? Do I need to do some shallow charge cycles or something?
I switched to Lifepo4 for greater range and power. 5 miles ain't gonna cut it.
Maybe I didn't charge long enough? Should the first charge time be longer than 10 hours?
Also: Another topic, mechanical: I saw something in here about a Torque Arm. Do I need one?