Congrats Marty! How I love the smell of entrepreneurs in the morning... 

1 boat load :wink:nicobie said:Curious how many you had to buy?
How to measure 5% salt in a spray bottle? Mix salt with hot water. How much salt?The apparatus for testing consists of a closed testing chamber, where a salted solution (mainly, a solution of 5%sodium chloride) is atomized by means of a nozzle.
1
Measure 5.0 grams, or 0.18 ounces, of table salt on a balance. Then, transfer the salt to a 4-ounce or larger container.
2
Measure 95 mL of distilled water using a 100-mL graduated cylinder, or 3.2 fluid ounces using a an 8-ounce measuring cup. Add the water to the container with the salt.
3
Cap the container with the salt solution and shake it until all of the salt has dissolved. The solution contains 5.0 grams of salt with a total solution mass of 100 grams. Therefore, weight percent = (5 grams) / (100 grams) * 100 = 5.0 percent salt.
Read more: How to Make a Five Percent Solution With Salt | eHow.com http://www.ehow.com/how_8076940_make-five-percent-solution-salt.html#ixzz2K5H1T2KG
liveforphysics said:Normal grades of stainless still rust. You really do want Monel if you don't want it to be staining ugly rust drips after a year or two.
Still offered for some stapler sizes:
http://www.arrowfastener.com/product/t50-monel-staples-item-506m1
JerZA80 said:Hi Marty: I sent you a PM inquiring about these staples. I'm not sure if you receive private messages but I was wondering if these are still available and how I would go about ordering. Did you ever put an ad on Ebay? Thanks