So I decided to beef up my motor mounts by welding it to the bottom of the battery tray. Also, being that I originally purchased these motor mounts they drilled the holes way too big for the connecting bolts so I’ve welded an additional plate to strengen up that area, but it also helps connect the battery tray to the motor mounts.
This image is before adding the additional plate for reinforcement. You can see the hole was drilled way too big in the motor mounts. I guess they did that so it fits multiple bikes, but would’ve much preferred to drill my own holes.
So will add these plates to reinforce.
Then here’s the plate connected with the bolt, but not welded at this point.
Here’s the motor mount without the bracket as you can see it’s just way too big of a hole.
Here’s everything, prepped and ready to weld!
![8D654FE2-E1AF-401E-B5B1-1F6BAA1E725A.jpeg 8D654FE2-E1AF-401E-B5B1-1F6BAA1E725A.jpeg](https://endless-sphere.com/sphere/data/attachments/208/208635-3f472edc6a34e4d857ae82e1d0e0f4d5.jpg)
Here’s a close-up you can see I left a little shoulder sticking out so I could build up the Weld bead
Here’s everything welded together!
![57257BB1-CBEF-42D3-BFF6-8CDCB389F7A5.jpeg 57257BB1-CBEF-42D3-BFF6-8CDCB389F7A5.jpeg](https://endless-sphere.com/sphere/data/attachments/208/208643-a54a3fc1dfd6b848704ebfe0166b70f5.jpg)
Not perfect welding, but should hold up just fine
![AC800F32-3887-4553-80F7-2BB40B6DCB0B.jpeg AC800F32-3887-4553-80F7-2BB40B6DCB0B.jpeg](https://endless-sphere.com/sphere/data/attachments/208/208644-bb97643349463283b5bb1f4e66690182.jpg)
Here’s the reinforcement plate welded.
This was actually my very first stick welding job I’ve done. I’ve used Mig once back in the day for auto bodywork but Man is there a learning curve with trying to arc weld/stick weld. Had to practice for several hours before I could figure out how to maintain the arc. So thankful for YouTube welding videos!
Oh, here’s a pic of my cheap welding set up. You can get this stick welder on Amazon for about 100 bucks not bad at all. It also does lift TIG. Comes with a power adapter you can plug into 110 V outlet.
But yeah, I went this route just because it was cheap. I don’t feel like spending to much money on a true welding set up with gas.
Had to pause on the battery assembly because the battery is pretty much being built into the Bike so needed to make sure that these motor mounts were beefed up enough since a lot of the weight will be sitting directly on top of the motor. Lots of thoughts and planning in this build.
Up Next I will weld some angle iron around the bottom of the battery tray.
![4ADCA08A-9EB2-4D88-92EF-666718BCC51D.jpeg 4ADCA08A-9EB2-4D88-92EF-666718BCC51D.jpeg](https://endless-sphere.com/sphere/data/attachments/208/208651-9cf24d95b45740e7f5824f8c28eb57d0.jpg)
That’ll give me connecting points so I can build a shield around the battery. Originally I was going to go with metal shield, but I might end up using carbon fiber sheets that are premade. They come 5 mm thick which should be strong enough for impacts. The carbon fiber would look a lot better than a metal shield because the metals gonna scratch every time you hit a rock so the carbon fiber might be the best solution, still brainstorming on ideas, but I’m not to that exact step yet.