ive been making golf trolley batteries for my dads golfing mates out of (2000mah) 18650 lipo cells. essentially 3s lipos as replacements, either an 3s4p (18 hole) or a 3s8p (36hole)
my batteries work fine in other trollies with lead acid or lipo controllers so this isnt a "my batteries don't have enough Ah issue".
annoyingly older powakaddy trollies use a 4s lifepo4 battery. meaning one of my fully charged lipos shows "low" on the trolley charge indicator from the start then about 13 holes into the course the low voltage cutout appears to be tripping despite the new battery still being good to go.
i see i have a few options
1. buy larger capacity lipo 18650s at great expense and hope the extra amp hours will make it round the 18 holes.
2. buy lifepo4 18650 cells at great expense then turn them into 4s.
3. use my existing stock of 2000mah lipos but adapt the batteries to 4s
4. any better ideas you guys have
im feeling option 3 as i have the parts so i dont have to wait for snail mail and its the least cost to me.
however i would like to ask if anyone knows if a 4s lipo batteries voltage will do any damage to a powakaddy controller??
if it is ok, i know the power gauge will show full almost constantly making it redundant but that is ok/acceptable.
thanks in advance for the advice
jim
my batteries work fine in other trollies with lead acid or lipo controllers so this isnt a "my batteries don't have enough Ah issue".
annoyingly older powakaddy trollies use a 4s lifepo4 battery. meaning one of my fully charged lipos shows "low" on the trolley charge indicator from the start then about 13 holes into the course the low voltage cutout appears to be tripping despite the new battery still being good to go.
i see i have a few options
1. buy larger capacity lipo 18650s at great expense and hope the extra amp hours will make it round the 18 holes.
2. buy lifepo4 18650 cells at great expense then turn them into 4s.
3. use my existing stock of 2000mah lipos but adapt the batteries to 4s
4. any better ideas you guys have
im feeling option 3 as i have the parts so i dont have to wait for snail mail and its the least cost to me.
however i would like to ask if anyone knows if a 4s lipo batteries voltage will do any damage to a powakaddy controller??
if it is ok, i know the power gauge will show full almost constantly making it redundant but that is ok/acceptable.
thanks in advance for the advice