Tiberius
10 kW
Well, I have just taken the plunge and ordered some Headway cells.
So far it has been easy and pleasant to deal with them directly. Victoria always answered my emails promptly and dealt with any technical questions.
BTW, I have ordered 38120L cells (10 Ah) rather than the 38120P (8 Ah but higher discharge rate). At 5C continuous, 10C peak, the L version looks as if it has enough current capacity.
Headway are also going to add tabs and weld them up into packs to my specification. Interestingly, this only increases the cost per cell by a small amount, but it has made a significant difference to the shipping cost.
Like Jeremy, I had to wire money to a Chinese bank, which adds to the cost and requires a bit of trust.
Nick
So far it has been easy and pleasant to deal with them directly. Victoria always answered my emails promptly and dealt with any technical questions.
BTW, I have ordered 38120L cells (10 Ah) rather than the 38120P (8 Ah but higher discharge rate). At 5C continuous, 10C peak, the L version looks as if it has enough current capacity.
Headway are also going to add tabs and weld them up into packs to my specification. Interestingly, this only increases the cost per cell by a small amount, but it has made a significant difference to the shipping cost.
Like Jeremy, I had to wire money to a Chinese bank, which adds to the cost and requires a bit of trust.
Nick