I'm confused. What kind of issues is mcmaster talking about for this bronze tinted polycarbonate sheeting?
http://www.mcmaster.com/#87245K114
Color: See below
Temperature Range: -40° to 200° F
Softening Temperature: 295° F
Tensile Strength: Good
Impact Strength: Excellent
Poor electrical insulator
Use indoors and outdoors
Machine with high-speed steel tooling
Hardness: Not rated