I just bought a $20, 6-year-old Panasonic battery.
I checked with a multimeter, nothing on output, the charging cable input on the BMS I get 54 V
I would like to check each cell group. The only battery I repaired before the batteries were at right angles to this one so it was a lot easier as I could see the sides
last time I unplugged the 14-pin socket and put a pin in each hole to get voltage. I can see where each wire comes from the battery, not sure where to measure the other side.
I think the battery is ok since I get 54 V, and it's a bad BMS I once changed a BMS, and the 14 pin socket was the same so easy job
I would greatly appreciate any steps to test the battery.
I checked with a multimeter, nothing on output, the charging cable input on the BMS I get 54 V
I would like to check each cell group. The only battery I repaired before the batteries were at right angles to this one so it was a lot easier as I could see the sides
last time I unplugged the 14-pin socket and put a pin in each hole to get voltage. I can see where each wire comes from the battery, not sure where to measure the other side.
I think the battery is ok since I get 54 V, and it's a bad BMS I once changed a BMS, and the 14 pin socket was the same so easy job
I would greatly appreciate any steps to test the battery.