Wow. That would suck! X-lyte is like the foundation.
 
Electric bike kit demand is at an all time high. It is not uncommon for a boom time in business to badly affect quality control. It has even happened to Toyota. Manufacturers up production by overworking their resources. The result is more problems with the products.
 
Maybe I'm lucky 'cause it ain't my good looks but my stuff is doing fine. Having drowned my 5304 a couple of weeks ago I ordered and received a new motor and controller from Electric Rider with no delays and no problems. Turns out I don't need the motor and will try and send it back this week but the new controller is nicer than the old one with smoother starts and the built in heat sink on the case. I have NO problems with Crystalyte quality except I sincerely wish they were waterproof.