I have an MXUS 4503 on the SB Cruiser trike that needs a bit of rework. (I've already welded a new end to the axle that had broken off)
Pics of the insides at the end of the post.
First, it has a fixable short between one of the "blue" phase windings and the stator lamination; I've temporarily fixed that by inserting plastic shims (bits of ziptie) between the winding and the face of the lamininations in the area that tapping the windings while running an isolation tester at 250v indicated a problem.
Second, I need to replace phase wires with something signficantly better than 18g but with very good insulation that has good thermal resistance to melting or softening.
I've poked around a number of threads discussing various varnish types and motor repair; some have links that still work, and I've found a number of different types of brush on, spray on, etc., insulating varnish. They all appear to be very similar, as do most of the ones discussed previously. But before I buy one, I would like opinions from those that have used similar types.
--is it likely that these (see links below) will flow down into the windings, and get between the stator and windings, to help create better insulation that what's there, potentially fixing this motor in a more permanent way (without rewinding, which is simply never going to happen)?
Secondarily, for the phase wires, I've been considering using magnet wire out of an old microwave oven transformer, or the transformer out of my first (dead) welder. But i'd also wnat to use something additional for insulation between each of the phases, and between the phases and the axle/bearing/etc. I suspect Kapton tape would be sufficient for this, as long as the temperatures can be kept down (with the 18g wire I could fit (that failed) temperatures witin hte wire jacket just outisde the axle were up to about 125-130F with 100A phase currents on the SFOC5 controller.
I need something reliable, that can handle 150-200A+ phase currents, for short bursts at least (a few seconds at a time, repeatedly over a few minutes of rding on my commutes, and longer times on other trips, with longer burst durations if carrying heavy cargo or a trailer full of dog, etc.
So...suggestions? Thoughts?
I'm looking to do this stuff in the next several days, depending on when the stuff will arrive here, once I have enough useful responses.
Kapton links first, then varnish:
https://www.amazon.com/Mil-Kapton-Tape-Polyimide-Yds/dp/B006ZFQNT6
https://www.amazon.com/Mil-Kapton-Tape-Polyimide-yds/dp/B006ZFNB2I
https://www.ebay.com/bhp/kapton-tape
https://www.amazon.com/dp/B008OA7CAE?psc=1&pf_rd_p=bb9788eb-24d0-484f-bb96-c8eca0708597&pf_rd_r=7VT9MQZ3KSEK8AWYH0JG&pd_rd_wg=5z5jI&pd_rd_i=B008OA7CAE&pd_rd_w=PH8KU&pd_rd_r=d328b2b1-00f8-4903-8951-a78f1ecdc165&ref_=pd_luc_rh_crh_rh_sim_03_01_t_img_lh
https://www.amazon.com/IEC-60317-50-Ed-1-0-Specifications/dp/B000Y2SGZ0/ref=sr_1_2?keywords=winding+varnish&qid=1552194033&s=gateway&sr=8-2
https://www.amazon.com/MG-Chemicals-GLPT-Insulating-Varnish/dp/B008OA7DDK/ref=sr_1_1?keywords=winding+varnish&qid=1552194033&s=gateway&sr=8-1
https://www.amazon.com/dp/B0034D1ZCM?psc=1&pf_rd_p=c35a81db-c1c9-4121-b93f-97ef6cbb19f8&pf_rd_r=7VT9MQZ3KSEK8AWYH0JG&pd_rd_wg=5z5jI&pd_rd_i=B0034D1ZCM&pd_rd_w=ZOuYx&pd_rd_r=d328b2b1-00f8-4903-8951-a78f1ecdc165&ref_=pd_luc_rh_crh_rh_sbs_02_04_t_img_lh
https://www.ebay.com/itm/MG-Chemicals-4228-225ML-Red-GLPT-Insulating-Varnish-225ML-Bottle/331529483474?epid=9011367709&hash=item4d30b274d2:g
OMAAOSwqu9VLBIl
https://www.ebay.com/itm/MG-Chemicals-4228-55ML-Red-GLPT-Insulating-Varnish-55ml-Bottle-NEW/231070150546?epid=11024539531&hash=item35ccdaaf92:g:13wAAOxygLxSVGYX
https://www.ebay.com/itm/MG-Chemicals-4228-1L-Red-GLPT-Insulating-Varnish-1-Liter-Bottle/251918313995?epid=659490270&hash=item3aa7806a0b:g:mFUAAOSwBahVLBM5
https://www.ebay.com/itm/MG-Chemicals-4228-55ML-Red-Insulating-Varnish-55-mL-Bottle/183674349887?epid=18012068013&hash=item2ac3d8293f:g:-dsAAOSwtM9cXBks:sc:ShippingMethodExpress!85051!US!-1
https://www.ebay.com/itm/GC-ELECTRONICS-10-9002-A-ANTI-OXIDATION-RED-INSULATING-VARNISH-2FL-OZ-BOTTLE/401087906220?epid=2254360029&hash=item5d62b3c1ac:g:NKoAAOSwr7ZW5b30:sc:USPSFirstClass!85051!US!-1
https://www.ebay.com/itm/MG-Chemicals-4226-55ML-Super-Corona-Dope-High-Voltage-Insulating-Varnish/120798757392?hash=item1c202ac210:g:RUAAAOSw-31bavzY
https://www.ebay.com/itm/MG-Chemicals-4228-55ML-Red-Insulating-Varnish/111653147651?hash=item19ff0bd403:g:ONEAAOSwwstbav74
https://www.ebay.com/itm/MOTOR-WINDING-TRANSFORMER-BARE-WIRE-INSULATING-VARNISH-SPRAY-REPAIR-COATING-CAN/152021663167?hash=item2365327dbf:g:YykAAOxyOypSWx3F
More details, pics, etc
https://endless-sphere.com/forums/viewtopic.php?f=2&t=67833&p=1450682#p1450462
Pics of the insides at the end of the post.
First, it has a fixable short between one of the "blue" phase windings and the stator lamination; I've temporarily fixed that by inserting plastic shims (bits of ziptie) between the winding and the face of the lamininations in the area that tapping the windings while running an isolation tester at 250v indicated a problem.
Second, I need to replace phase wires with something signficantly better than 18g but with very good insulation that has good thermal resistance to melting or softening.
I've poked around a number of threads discussing various varnish types and motor repair; some have links that still work, and I've found a number of different types of brush on, spray on, etc., insulating varnish. They all appear to be very similar, as do most of the ones discussed previously. But before I buy one, I would like opinions from those that have used similar types.
--is it likely that these (see links below) will flow down into the windings, and get between the stator and windings, to help create better insulation that what's there, potentially fixing this motor in a more permanent way (without rewinding, which is simply never going to happen)?
Secondarily, for the phase wires, I've been considering using magnet wire out of an old microwave oven transformer, or the transformer out of my first (dead) welder. But i'd also wnat to use something additional for insulation between each of the phases, and between the phases and the axle/bearing/etc. I suspect Kapton tape would be sufficient for this, as long as the temperatures can be kept down (with the 18g wire I could fit (that failed) temperatures witin hte wire jacket just outisde the axle were up to about 125-130F with 100A phase currents on the SFOC5 controller.
I need something reliable, that can handle 150-200A+ phase currents, for short bursts at least (a few seconds at a time, repeatedly over a few minutes of rding on my commutes, and longer times on other trips, with longer burst durations if carrying heavy cargo or a trailer full of dog, etc.
So...suggestions? Thoughts?
I'm looking to do this stuff in the next several days, depending on when the stuff will arrive here, once I have enough useful responses.
Kapton links first, then varnish:
https://www.amazon.com/Mil-Kapton-Tape-Polyimide-Yds/dp/B006ZFQNT6
https://www.amazon.com/Mil-Kapton-Tape-Polyimide-yds/dp/B006ZFNB2I
https://www.ebay.com/bhp/kapton-tape
https://www.amazon.com/dp/B008OA7CAE?psc=1&pf_rd_p=bb9788eb-24d0-484f-bb96-c8eca0708597&pf_rd_r=7VT9MQZ3KSEK8AWYH0JG&pd_rd_wg=5z5jI&pd_rd_i=B008OA7CAE&pd_rd_w=PH8KU&pd_rd_r=d328b2b1-00f8-4903-8951-a78f1ecdc165&ref_=pd_luc_rh_crh_rh_sim_03_01_t_img_lh
https://www.amazon.com/IEC-60317-50-Ed-1-0-Specifications/dp/B000Y2SGZ0/ref=sr_1_2?keywords=winding+varnish&qid=1552194033&s=gateway&sr=8-2
https://www.amazon.com/MG-Chemicals-GLPT-Insulating-Varnish/dp/B008OA7DDK/ref=sr_1_1?keywords=winding+varnish&qid=1552194033&s=gateway&sr=8-1
https://www.amazon.com/dp/B0034D1ZCM?psc=1&pf_rd_p=c35a81db-c1c9-4121-b93f-97ef6cbb19f8&pf_rd_r=7VT9MQZ3KSEK8AWYH0JG&pd_rd_wg=5z5jI&pd_rd_i=B0034D1ZCM&pd_rd_w=ZOuYx&pd_rd_r=d328b2b1-00f8-4903-8951-a78f1ecdc165&ref_=pd_luc_rh_crh_rh_sbs_02_04_t_img_lh
https://www.ebay.com/itm/MG-Chemicals-4228-225ML-Red-GLPT-Insulating-Varnish-225ML-Bottle/331529483474?epid=9011367709&hash=item4d30b274d2:g
https://www.ebay.com/itm/MG-Chemicals-4228-55ML-Red-GLPT-Insulating-Varnish-55ml-Bottle-NEW/231070150546?epid=11024539531&hash=item35ccdaaf92:g:13wAAOxygLxSVGYX
https://www.ebay.com/itm/MG-Chemicals-4228-1L-Red-GLPT-Insulating-Varnish-1-Liter-Bottle/251918313995?epid=659490270&hash=item3aa7806a0b:g:mFUAAOSwBahVLBM5
https://www.ebay.com/itm/MG-Chemicals-4228-55ML-Red-Insulating-Varnish-55-mL-Bottle/183674349887?epid=18012068013&hash=item2ac3d8293f:g:-dsAAOSwtM9cXBks:sc:ShippingMethodExpress!85051!US!-1
https://www.ebay.com/itm/GC-ELECTRONICS-10-9002-A-ANTI-OXIDATION-RED-INSULATING-VARNISH-2FL-OZ-BOTTLE/401087906220?epid=2254360029&hash=item5d62b3c1ac:g:NKoAAOSwr7ZW5b30:sc:USPSFirstClass!85051!US!-1
https://www.ebay.com/itm/MG-Chemicals-4226-55ML-Super-Corona-Dope-High-Voltage-Insulating-Varnish/120798757392?hash=item1c202ac210:g:RUAAAOSw-31bavzY
https://www.ebay.com/itm/MG-Chemicals-4228-55ML-Red-Insulating-Varnish/111653147651?hash=item19ff0bd403:g:ONEAAOSwwstbav74
https://www.ebay.com/itm/MOTOR-WINDING-TRANSFORMER-BARE-WIRE-INSULATING-VARNISH-SPRAY-REPAIR-COATING-CAN/152021663167?hash=item2365327dbf:g:YykAAOxyOypSWx3F
More details, pics, etc
https://endless-sphere.com/forums/viewtopic.php?f=2&t=67833&p=1450682#p1450462