torqueboards
1 MW
Hi guys,
Please tell me what you think. Would care to hear your opinions and suggestions.
I am more thinking of the board on the right side. The board is 39.5" and 9.75" width.
I've also redesigned my current bolt on to be with M6 bolts.. However, in the process of re-designing a complete carbon fiber board I decided to build from the ground up. I realize for the motor mounts that I never planned on using a belt cover, motor pulley cover or any motor protective plate. In the end, for myself they just add to more complication, more weight, more cost. Very simple and easy to build is a better option. Here is picture of the dual rear with 12mm pulleys.
Here is a photo of the top of the deck with the battery pack. It's a 10S3P pack. I may change to 12S3P but it tends to run bigger but I think 10S is ok since it's cheaper, flatter and not as long.
For the height of the deck, I wanted a drop through so it's real low to the ground.
Personally, I also want a mini deck.. This one is 30" long.
Mini - Style 1
Mini - Style 2 (Jet Board)
What do you guy's think?
The idea for the build is 10S3P, Dual VESC, 6355 230KV (I like the faster motors, they go 20-25% inclines much easier), 12mm belt setup.
Please tell me what you think. Would care to hear your opinions and suggestions.
I am more thinking of the board on the right side. The board is 39.5" and 9.75" width.

I've also redesigned my current bolt on to be with M6 bolts.. However, in the process of re-designing a complete carbon fiber board I decided to build from the ground up. I realize for the motor mounts that I never planned on using a belt cover, motor pulley cover or any motor protective plate. In the end, for myself they just add to more complication, more weight, more cost. Very simple and easy to build is a better option. Here is picture of the dual rear with 12mm pulleys.

Here is a photo of the top of the deck with the battery pack. It's a 10S3P pack. I may change to 12S3P but it tends to run bigger but I think 10S is ok since it's cheaper, flatter and not as long.

For the height of the deck, I wanted a drop through so it's real low to the ground.


Personally, I also want a mini deck.. This one is 30" long.
Mini - Style 1


Mini - Style 2 (Jet Board)

What do you guy's think?
The idea for the build is 10S3P, Dual VESC, 6355 230KV (I like the faster motors, they go 20-25% inclines much easier), 12mm belt setup.