I saw recently post about Musk offering power solutions to Australia, saying 250 dollars per kWh
So thats 125 dollars per 500Wh
But 500Wh Yamaha battery costs 700 euro, that is 742 dollars and that is about 6x more expensive !!!!!!
WHY? Why is this small ebike battery without supercharging, watercooling, more expensive ?
Where is the problem?I am sure 40 cells that they put there cost them 100 euro, thats how much would cost Panasonic cells 18650 PF.
Can I not somehow connect other Pannasonic Battery pack to my Yamaha ebike?
This is the only reason i regret purchasing my Yamaha ebike, its great, it climbs every hill, but the battery capacity is low, charging is slow, 3,5hours....
I am considering buying another battery for long trips, but hey, for the 700 euro ?!
400Wh option i found for 480 euro .....thats still not a big win at all!
Please help, suggestions please, i am planning long trips arround Europe, and after going Asia on my ebike! Hopefully ill get chargers regularly on my way
So thats 125 dollars per 500Wh
But 500Wh Yamaha battery costs 700 euro, that is 742 dollars and that is about 6x more expensive !!!!!!
WHY? Why is this small ebike battery without supercharging, watercooling, more expensive ?
Where is the problem?I am sure 40 cells that they put there cost them 100 euro, thats how much would cost Panasonic cells 18650 PF.
Can I not somehow connect other Pannasonic Battery pack to my Yamaha ebike?
This is the only reason i regret purchasing my Yamaha ebike, its great, it climbs every hill, but the battery capacity is low, charging is slow, 3,5hours....
I am considering buying another battery for long trips, but hey, for the 700 euro ?!
400Wh option i found for 480 euro .....thats still not a big win at all!
Please help, suggestions please, i am planning long trips arround Europe, and after going Asia on my ebike! Hopefully ill get chargers regularly on my way