Some Update:
up to 5,5KW Regen eBrake killed a bunch of spokes.
so i did it also....change to motorcycle spokes and shinko SR241.
6 Hours of Lacing my first Wheel. 3 of them to true the wheel. I drilled the Cromotor Spoke Holes to 4mm.
Spokes i only found in 9g (4mm) Was tired of Searching also.
Rim is an Excel 19x1.4...it was a special order. No way to find another Rim in Black. ProWheels was out of Stock + Shipping to Germany
is near same Expensive. I hope that i never get any Problems with that Wheel/Rim/Spokes.....(now...)
The Wheel is true enough for me....wobbles 1mm in each direction. The Tyre wobbles alot more.
tried it 3 Times to fix that.....No Success. On Driving i dont feel that. But i hate it when i know theres something not that perfect i like....
Bare Motor with Rim has now 13,4Kg
Incl Tire 17Kg (!)....Heavy...Backwheel alone weights same as a complete ebike *lol
But Thx to all who postet tyre stuff to help me finding the right parts.
...special thx goes out to Rix to be my spoke calculator ;P
Some Pics:
up to 5,5KW Regen eBrake killed a bunch of spokes.
so i did it also....change to motorcycle spokes and shinko SR241.
6 Hours of Lacing my first Wheel. 3 of them to true the wheel. I drilled the Cromotor Spoke Holes to 4mm.
Spokes i only found in 9g (4mm) Was tired of Searching also.
Rim is an Excel 19x1.4...it was a special order. No way to find another Rim in Black. ProWheels was out of Stock + Shipping to Germany
is near same Expensive. I hope that i never get any Problems with that Wheel/Rim/Spokes.....(now...)
The Wheel is true enough for me....wobbles 1mm in each direction. The Tyre wobbles alot more.
tried it 3 Times to fix that.....No Success. On Driving i dont feel that. But i hate it when i know theres something not that perfect i like....
Bare Motor with Rim has now 13,4Kg
Incl Tire 17Kg (!)....Heavy...Backwheel alone weights same as a complete ebike *lol
But Thx to all who postet tyre stuff to help me finding the right parts.
...special thx goes out to Rix to be my spoke calculator ;P
Some Pics:
![2014-09-18%2020.02.32.jpg](/sphere/proxy.php?image=https%3A%2F%2Fdl.dropboxusercontent.com%2Fu%2F55508799%2Febike%2Fraptor%2F2014-09-18%252020.02.32.jpg&hash=fc411501b3457ffca29d5b72004f2f56)
![2014-09-18%2012.58.54.jpg](/sphere/proxy.php?image=https%3A%2F%2Fdl.dropboxusercontent.com%2Fu%2F55508799%2Febike%2Fraptor%2F2014-09-18%252012.58.54.jpg&hash=e31e21f3a21f5b6acd4962f94f42b9d1)
![2014-09-18%2013.48.55.jpg](/sphere/proxy.php?image=https%3A%2F%2Fdl.dropboxusercontent.com%2Fu%2F55508799%2Febike%2Fraptor%2F2014-09-18%252013.48.55.jpg&hash=342905a3422c7550ef63f64343f9d15f)