18650 battery building, complete process recorded on live!

Nobuo

10 kW
Joined
Nov 21, 2014
Messages
839
Location
Madrid
I always share my on live battery buildings on ES Facebook group, I received petitions to share here also in order to show to the rest of the community. So here are the last broadcasting!
Unfortunately they have an expiration time of 24hours, I hope you enjoy :eek:
(If you can't see the video within the 24 hours on the computer, you are able to see into Periscope app on your phone, always within 24h)

part 1: spot soldering ---> https://www.periscope.tv/w/aLyZSzM3ODg4MzF8MUJkR1lsUU53a01LWEPprlir0FtpnG50uNJZOSukK7P-5yII4uFGNQdQcd29

part 2: BMS, wiring, connectors. ---> https://www.periscope.tv/w/aLy5ezM3ODg4MzF8MVprS3pETEVOcXFKdiBNzHZnnTr6_WN_cCny3EHW2xe9uBT07AI080wkd-_1

part 3: capacity meter, shrink wrapping and waterproof sealing ---> https://www.periscope.tv/w/aL2gRzM3ODg4MzF8MVJER2xlUWdla05KTAE47-rXcoW41y1iRf-Bd-pKrMFFQT2dYWo1-f5Jllgy

The best parts are any small mishaps that happen on live. For example in part 3, you can see that because of excessive heat when wrapping the insulation cover, the shrink wrap broke on a small hole on a side while heating, it teaches to be concerned about dropping the heat with a little caution and dosed, and indeed that everything could happen broadcasting!
 
In some computers (web browsers indeed) the video doesn't work properly, and you only can hear it for example. With Windows 7 or more and Chrome browser it works on the computer, I don't know in which other browser could work good.

It works always on the Periscope app, it is very light, not adds or anything undesired. https://www.periscope.tv/
 
The video works here, on my PC with Chrome.
But without the possibility to fast forward or jump.. it kinda kills the fun.
 