SkyknightJohn
100 W
*fixed! Thanks.Hyena said:I assume those weights are backwards and that the 1.4 is lighter?
I was surprised at the difference as well, but I'm guessing it's because you make it wider in the middle, meaty section of the rim, adding a fair bit of material. I can't vouch for the accuracy of the scales I used, they're just old postal scales at work.Their limits are 5 lbs / 2.2 kg.
At the power levels you run, I would go fatter too. I'm still low and slow, so every bit helps. (says the man with an 85 lb. bike... 8) )Hyena said:I like the wider rims myself. Fat is Phat
Ha Ha! Well, that's only because I couldn't get a 36h 19x1.4 in red.Rix said:Glad you did it with different colored rims