Any1 else stumble across these ? it says 2000 cycles in the data sheet and not at some .2c discharge but at 1c. 70% capacity at 2000 cycles. The vendor is in Utah.
http://electriccarinternational.com/page52.php
http://electriccarinternational.com/media/img-prod/Pure-EVS-XC-CPM-PHEV-30Ah-Power-Lithium-Electric-Car-EV-Battery-small.jpg
Pouch Lithium EV Batteries
Pure EVS POWER and ENERGY Pouch Batteries
Pure-EVS-XC-CPM-PHEV-30Ah-Power-Lithium-electric-car-ev-battery
30Ah POWER, 20C, 3.7V
LiMin204
W x H x L
.47 x 6.9 x 13.2in
12 x 161 x 272mm
$132 each
Pulse Discharge Current (≤30sec) ≤600A (20C)
Factory will assemble any serial or parallel configuration of these batteries for free.
They also have 3c 30 ah pouches for $90 that gets 2000 cycles at 1c
and another 3c 30 ah pouch for $59 that gets 1500 cycles at 1c
http://electriccarinternational.com/page52.php
http://electriccarinternational.com/media/img-prod/Pure-EVS-XC-CPM-PHEV-30Ah-Power-Lithium-Electric-Car-EV-Battery-small.jpg
Pouch Lithium EV Batteries
Pure EVS POWER and ENERGY Pouch Batteries
Pure-EVS-XC-CPM-PHEV-30Ah-Power-Lithium-electric-car-ev-battery
30Ah POWER, 20C, 3.7V
LiMin204
W x H x L
.47 x 6.9 x 13.2in
12 x 161 x 272mm
$132 each
Pulse Discharge Current (≤30sec) ≤600A (20C)
Factory will assemble any serial or parallel configuration of these batteries for free.
They also have 3c 30 ah pouches for $90 that gets 2000 cycles at 1c
and another 3c 30 ah pouch for $59 that gets 1500 cycles at 1c