48v15ah Ping
Ebikes 25amp controller set up matched to a 9c
I had been experiencing some problems with short out the past couple weeks, prime suspect was at the discharge wires, the metal contacts looked corroded. I figured I'd just deal with it because anderson crimpers are pricey.
Well, today I went to pull the battery out to charge and I couldn't pull the discharge wires apart from the controller, the plastic housings had melted together I was eventually able to pry it off, but that pretty much settled the issue of when I deal with this problem. I guess the corroded contacts just got that hot, no other idea how that could happen.
So word of caution, if you are getting short outs, replace the connections , they can melt
Ebikes 25amp controller set up matched to a 9c
I had been experiencing some problems with short out the past couple weeks, prime suspect was at the discharge wires, the metal contacts looked corroded. I figured I'd just deal with it because anderson crimpers are pricey.
Well, today I went to pull the battery out to charge and I couldn't pull the discharge wires apart from the controller, the plastic housings had melted together I was eventually able to pry it off, but that pretty much settled the issue of when I deal with this problem. I guess the corroded contacts just got that hot, no other idea how that could happen.
So word of caution, if you are getting short outs, replace the connections , they can melt