drunkencat129
100 W
- Joined
- Aug 5, 2008
- Messages
- 116
UPDATE BELOW
oke guys i was messing around when i got the idea to mod the spair battery medics i got to disscharge and balance better and faster so far i moded them cheaply only cost 5$ for the 6.2ohm 4w metal oxide resisters i made it so it can be removed and pluged in if needed its a plug in mod so far i found it takes 30 min to take a 4400ah lipo from 4.2v to 4.0v it gets hot but not to crazy hot its about same temp as the old diy 24ch bms on for forums
best part with thiss mod cases can stay oem except for 2 holes in the sides for the extra wires to attach the the resisters i added to the board
next im going to mod a heat sink to them ^_^ thermal epoxy needs to be found so far found a small tube for 60$ but its only enouf for one board
here is the link to the resisters i got on ebay http://www.ebay.ca/itm/230584620519?ssPageName=STRK:MEWNX:IT&_trksid=p3984.m1439.l2649
here are the pics enjoy
the tester ^_^
the finished product
oke guys i was messing around when i got the idea to mod the spair battery medics i got to disscharge and balance better and faster so far i moded them cheaply only cost 5$ for the 6.2ohm 4w metal oxide resisters i made it so it can be removed and pluged in if needed its a plug in mod so far i found it takes 30 min to take a 4400ah lipo from 4.2v to 4.0v it gets hot but not to crazy hot its about same temp as the old diy 24ch bms on for forums
best part with thiss mod cases can stay oem except for 2 holes in the sides for the extra wires to attach the the resisters i added to the board
next im going to mod a heat sink to them ^_^ thermal epoxy needs to be found so far found a small tube for 60$ but its only enouf for one board
here is the link to the resisters i got on ebay http://www.ebay.ca/itm/230584620519?ssPageName=STRK:MEWNX:IT&_trksid=p3984.m1439.l2649
here are the pics enjoy
the tester ^_^
the finished product