I have an Amazon spot welder for batteries. Is there a plastic tool thing or something that will hold the probes for me to keep the tips of the electrodes the same distance apart from each other the whole time, sort of like a one hand tool to hold the probes? Also is there a specific tool to keep the probes clean?
 
Do you have a 3d printer? If so, you could design something simple to hold them at, say, a 45 degree angle. I did that:
IMG_20240401_140950.jpg

As for cleaning the tips. I use a bench grinder or power drill with a brass brush every few hundred welds.
 
Do you have a 3d printer? If so, you could design something simple to hold them at, say, a 45 degree angle. I did that:
View attachment 361454

As for cleaning the tips. I use a bench grinder or power drill with a brass brush every few hundred welds.
Right, something like that. There's not a commercial product that I can buy that will hold them for me that I can get off like Amazon?

Interesting, brass bush. Probably good idea.