Hey everyone (im new here) ,i have a Bafang BBS02B which i've killed the controller (maybe cause it was programmed to 25 with 58.8v 14s battery but anyway) and im up to a ESC i can draw more amps than the original controller. I found one Flier "E-bike" controller 22s 400A so it can be reliable and future-proof my problem is that it does NOT have any current limiter , ive measured the resistance and the motor can draw up to 200amps . My battery cannot produce more than 70 and the motor wont last a hour with that kind of power . So i want to limit the amp in the esc (in the battery side mostly to be safe) does anyone have any idea ? Thanks