Doctorbass
100 GW
I am looking to install the low side FETs of my 36 fets controller direct on the heatsink bar without insulator and i am looking for the best ELECTRICAL and THERMAL conductive compound.
This time i can benefit of the great thermal conductibility of ELECTRICAL conductor material but i just found electical insulated material
The Artic Silver 5 is great.. but i think i can get better.. apparently the diamond powder or carbon powder based compound are good..
The Artic silver 5 is 7.5W/degree K / m.
Pure silver is 410.. so i guess there is a trade off between both right?
Any suggestions?
Doc
This time i can benefit of the great thermal conductibility of ELECTRICAL conductor material but i just found electical insulated material
The Artic Silver 5 is great.. but i think i can get better.. apparently the diamond powder or carbon powder based compound are good..
The Artic silver 5 is 7.5W/degree K / m.
Pure silver is 410.. so i guess there is a trade off between both right?
Any suggestions?
Doc