recumpence
1 GW
Here are a couple pics of some new CNC machined Lipo boxes we machined today.
I wanted some very durable boxes that can contain a lipo fire relatively well along with handling a fall off a bike. I also wanted to make sure the packs fit sung for two reasons;
#1 A snug fit helps increase the "C" rating of these cells allowong them to be pushed harder.
#2 A snug fit gives much better thermal transfer to keep the cells nice and cool.
They are machined from 6061 aluminum with covers held down with 6 screws. The inside dimentions are 6 inches by 4 inches wide by 2.060 inch deep. This gives a snug fit for the popular 25C Turnigy 6S packs we are using.
If anyone is interested, they are $95 per box. Oh, there are no wire holes drilled. That way each person can drill their own hole for wire exit either through the top, front, or bottom of the box. Admittedly, these were only made for my personal builds. However, I had time and material to make more than I need. So, I made a few extra.
These boxes are made for only two packs because I wanted to make sure any battery failure would only affect one other pack. This also allows easier mounting. It is easier to mount two or three smaller boxes than one large box.
Anyway, my builds will use these from now on. I will also be using them as controller cases. I can fit two HV160s in each box easily.
Matt
I wanted some very durable boxes that can contain a lipo fire relatively well along with handling a fall off a bike. I also wanted to make sure the packs fit sung for two reasons;
#1 A snug fit helps increase the "C" rating of these cells allowong them to be pushed harder.
#2 A snug fit gives much better thermal transfer to keep the cells nice and cool.
They are machined from 6061 aluminum with covers held down with 6 screws. The inside dimentions are 6 inches by 4 inches wide by 2.060 inch deep. This gives a snug fit for the popular 25C Turnigy 6S packs we are using.
If anyone is interested, they are $95 per box. Oh, there are no wire holes drilled. That way each person can drill their own hole for wire exit either through the top, front, or bottom of the box. Admittedly, these were only made for my personal builds. However, I had time and material to make more than I need. So, I made a few extra.
These boxes are made for only two packs because I wanted to make sure any battery failure would only affect one other pack. This also allows easier mounting. It is easier to mount two or three smaller boxes than one large box.
Anyway, my builds will use these from now on. I will also be using them as controller cases. I can fit two HV160s in each box easily.
Matt