I have a Sunrunner ebike that I got as non-working/dead battery.
The original battery is 24v 6Ah lifepo4 which I assume is 8s4p.
24v 10Ah lifepo4 is gonna cost £300, any smaller Ah don't provide enough current. 24v 10ah liion is £125
Can I buy a 24v 10ah li-ion standard battery and just drop in?
lifepo4 8s would operate 20.0v - 27.2v voltage range
liion 7s would be 21v - 29.4v
Is there a chance that would blow the controller? Does the controller run at reduced speed because it senses the battery voltage, which might give me issues because of the different voltage profiles of the cells?
I hooked it up to 21.8v and it operates the motor at low speed on the throttle, at 25.4v it went a little faster. This is with no load (wheel in the air) and running from nimh AAs just to test if it's worth spending more money on as I don't have an existing battery to test with.
The original battery is 24v 6Ah lifepo4 which I assume is 8s4p.
24v 10Ah lifepo4 is gonna cost £300, any smaller Ah don't provide enough current. 24v 10ah liion is £125
Can I buy a 24v 10ah li-ion standard battery and just drop in?
lifepo4 8s would operate 20.0v - 27.2v voltage range
liion 7s would be 21v - 29.4v
Is there a chance that would blow the controller? Does the controller run at reduced speed because it senses the battery voltage, which might give me issues because of the different voltage profiles of the cells?
I hooked it up to 21.8v and it operates the motor at low speed on the throttle, at 25.4v it went a little faster. This is with no load (wheel in the air) and running from nimh AAs just to test if it's worth spending more money on as I don't have an existing battery to test with.