MTH07
1 mW
I built a battery for my BBSHD powered bike in a 14s3p configuration using Samsung 25s 18650 cells and a Daly BMS (not smart BMS, just basic balancing unit).
After a short ride a few weeks ago depleting the battery to about 52 volts, I got home and forgot to unplug the battery from the bike. Apparently there is a significant phantom draw, and it drained the battery all the way to zero volts. The over-discharge protection did not appear to do its job at all. I initially thought it kicked in and opened the circuit, but it measures zero volts across the cells, and is confirmed dead.
I am going to build a replacement, and definitely will not be using a Daly BMS (likely either JK or JBD). But I am a little surprised about such a basic function on the Daly unit failing like that. I thought I would post on here and see if possible it was something I did incorrectly, or if other have had this experience with Daly BMS units. The battery worked great for a dozen or so rides/recharges, coming up to the right voltage and discharging consistently at the anticipated rate.
After a short ride a few weeks ago depleting the battery to about 52 volts, I got home and forgot to unplug the battery from the bike. Apparently there is a significant phantom draw, and it drained the battery all the way to zero volts. The over-discharge protection did not appear to do its job at all. I initially thought it kicked in and opened the circuit, but it measures zero volts across the cells, and is confirmed dead.
I am going to build a replacement, and definitely will not be using a Daly BMS (likely either JK or JBD). But I am a little surprised about such a basic function on the Daly unit failing like that. I thought I would post on here and see if possible it was something I did incorrectly, or if other have had this experience with Daly BMS units. The battery worked great for a dozen or so rides/recharges, coming up to the right voltage and discharging consistently at the anticipated rate.