999zip999
100 TW
Ok these my second edge 1,500 motor left sitting and broken for months. The first let it's magnets go. I triedtotake out unglued magnets on first motor as taking out the magnets they jumped and cracked. So ok second motor started scraping and just know pulled apart. WHAT unglued magnets ??? The first motor got hot the second no.
So I see that expoly JB weld hi temp 650% at the auto store. Looks good what you stink ?
Plus how is best to keep magnets in order. Plus help before I start. What arethe secrets ??? Cheap ass motor. I think it made those guys bankrupt for a while.
So I see that expoly JB weld hi temp 650% at the auto store. Looks good what you stink ?
Plus how is best to keep magnets in order. Plus help before I start. What arethe secrets ??? Cheap ass motor. I think it made those guys bankrupt for a while.