raylo32
🚴‍♂️ Mega poster
Just an FYI for folks who have an older King Shark which won't charge on a Grin Satiator unless you do a force start. While I was corresponding with EM3EV a couple weeks ago about another battery I mentioned that I did not like having to force start the Grin with the KS and Joseph sent me the latest firmware for the KS BMS that gets rid of the problem. If anyone here needs that file let me know and I can PM it to you. Alternatively, you can e-mail EM3EV and they will send it to you. You will also need the ALi BMS app to update the firmware which is available on the Apple App Store. Not sure about the Google PlayStore.