andreym
100 W
It was a loooong winter. Many things changed since
somebody probably saw my posts about cromotor. So today I finally managed to install rear brakes on GT.
here was the start of the rear brake- quest http://endless-sphere.com/forums/viewtopic.php?f=2&t=33831&p=535553&hilit=gustav#p535553
so here is the end of story A bit of filing of 2 adapters and viola sorry for crappy phone pictures.
it`s not so big clearance left but it works well though
also you may see one of torque arms - there are 3 of them total - each 4mm of stainless steel laser cut to fit 16mm of cromotor axle.
I hope 12mm total of torque arms would be enough
btw got my go-pro 2, so after the roars become dry more crazy videos to come
for now tried it only at the office (long hall there) it pulls wheelies easy at only 65amps at 75volts (half discharged 20s lipo)
somebody probably saw my posts about cromotor. So today I finally managed to install rear brakes on GT.
here was the start of the rear brake- quest http://endless-sphere.com/forums/viewtopic.php?f=2&t=33831&p=535553&hilit=gustav#p535553
so here is the end of story A bit of filing of 2 adapters and viola sorry for crappy phone pictures.
it`s not so big clearance left but it works well though
also you may see one of torque arms - there are 3 of them total - each 4mm of stainless steel laser cut to fit 16mm of cromotor axle.
I hope 12mm total of torque arms would be enough
btw got my go-pro 2, so after the roars become dry more crazy videos to come
for now tried it only at the office (long hall there) it pulls wheelies easy at only 65amps at 75volts (half discharged 20s lipo)