I have a Gio Falcon, brand new from dealer only 2 months old, this model ;
https://gvabrands.com/collections/electric-scooters/products/falcon
Has ben running great until yesterday, was out at a restaurant, battery was fully charged when I left
to go to restaurant, was only in place for 40 mins, when I came back out bike would not turn on.
No power, no horn, no lights, panel display did not power on
Ended up having to physically walk bike home, did not have pedals on bike at time.
On the way home, a couple of times there were hills, when I went down a hill, I could see the LED panel display with the
spedometer etc, LED battery charge visual display, signal light indicator, erratically light up - flashing on and off
but when at bottom of hill would all go dark again
When I got home tried to charge battery up, but it was close to full so it didnt charge long - tried turning it on again
and still nothing
Read manual trouble shooting section for things to try ;
opened bike seat and looked at fuse box, switch was turned to off position, I tried to turn it to the on position
and bike emitted a loud alarm sound, beeping, and then it switched it self back to the off position, fuse box will
not stay in the on position
called the dealer and they had no meaningful answers, they are a long ways away so its a real challenge for me to have to
port it back to them
any ideas as to why this is happening and how to fix?
I have a Gio Falcon, brand new from dealer only 2 months old, this model ;
https://gvabrands.com/collections/electric-scooters/products/falcon
Has ben running great until yesterday, was out at a restaurant, battery was fully charged when I left
to go to restaurant, was only in place for 40 mins, when I came back out bike would not turn on.
No power, no horn, no lights, panel display did not power on
Ended up having to physically walk bike home, did not have pedals on bike at time.
On the way home, a couple of times there were hills, when I went down a hill, I could see the LED panel display with the
spedometer etc, LED battery charge visual display, signal light indicator, erratically light up - flashing on and off
but when at bottom of hill would all go dark again
When I got home tried to charge battery up, but it was close to full so it didnt charge long - tried turning it on again
and still nothing
Read manual trouble shooting section for things to try ;
opened bike seat and looked at fuse box, switch was turned to off position, I tried to turn it to the on position
and bike emitted a loud alarm sound, beeping, and then it switched it self back to the off position, fuse box will
not stay in the on position
called the dealer and they had no meaningful answers, they are a long ways away so its a real challenge for me to have to
port it back to them
any ideas as to why this is happening and how to fix?