Yeah, if you guys don't mind checking, I'd love to see a photo of what it looks like when its not broken.
I'm trying to work out if it was just weak to begin with, or if it was just tacked in place with a couple of lousy welds...
Either way, it's certainly something you should keep an eye on. I suspect it was just poor design, and they never suspected that 90 kg fatties like me would ride it flat out everywhere I go, for 11,000+ km