got this battery for testing

heres a link for how to spot a fake HG2

https://batterybro.com/blogs/18650-wholesale-battery-reviews/104619270-can-you-identify-the-fake-lg-hg2-18650-battery

AKZMYO8.jpg


VtDLOiQ.jpg


fW6gTEq.jpg


the can has absolutely no identifiers on it

tLq0mrv.jpg


bftwHrD.jpg


insulator ring is textured on one side, you can see a bit of "shine" in between 12 and 1 o-clock but?

A5dR1Vh.jpg


weld marks are different than in the article

HIabylV.jpg


4cTQhqA.jpg


maybe its part of the 2016 batch mentioned in how to spot a fake

interupted my 30q test, dont mind the graph title

EcSZd4u.jpg


charged to 4.2v

kV7SIuU.png


battery held at 4.191v after 2 minutes :thumb: start 10amp discharge

HXqvAqf.png


stopped discharge at 3.2v, battery temp reached 128f/53.3 celsius

GiWw7n9.png


curve looks good, mah is about right, actually it should be around 1900/2000mah at 3.2v from the data sheet

https://www.nkon.nl/sk/k/hg2.pdf

ill get another hg2 tomorrow to compare

nVvkw64.jpg


ill do a 5amp discharge to 2.5v and compare to this chart

ANoDu9L.jpg


heres the 5amp discharge 2585mah, peak temp 110f

XwGuCA4.png


if you compare to this sites handy comparison charts, you can change discharge rates see curves and compare 2 batteries on same chart, i dont know what this battery is

https://lygte-info.dk/review/batteries2012/Common18650comparator.php
 
i "borrowed" a HG2 from a friends vape :D
did a 5amp discharge and the curve and capacity looks right
peeled the wrapper off and theres no markings on the can

5amp was 2738mah

zjlQJaF.png


go to lygte and this is the 5amp curve, 2750mah?

MNblGyM.png


going to run a few cycles at the same settings as the 30Q and vtc6

N1kp6hv.jpg


7dWSuZB.png


the wrapper has this warning on it

theshorelinemarket_2613_23066210.jpg

#01 d-2414, c-2372
#02 d-2408, c-2364
#03 d-2399, c-2355 changing wait time from 6/2 to 10/5 minutes
#04 d-2391, c-2347
#05 d-2385, c-2342
#06 d-2379, c-2336
#07 d-2374, c-2329
#08 d-2370, c-2327
#09 d-2366, c-2322
#10 d-2363, c-2321
#11 d-2361, c-2319
#12 d-2360, c-2318
#13 d-2359, c-2317 numbers have stabilized, removing wait times for continuous discharge/charge/cycle
#14 d-2357, c-2314
#15 d-2353, c-2310
#16 d-2353, c-2308
#17 d-2351, c-2307
#18 d-2349, c-2305
#19 d-2348, c-2304
#20 d-2347, c-2302
#21 d-2344, c-2301
#22 d-2344, c-2247 stopped test


heres a 18650 date code look up tool
https://batterybro.com/pages/18650-date-code-lookup-tool
 
In the mid-90s Macalester College, St. Paul, MN sponsored the publication of a new magazine entitled "Business Ethics" in cooperation with their MBA programs. Its small circulation never caught on with the business world. It only lasted a couple years.

Do you think it's possible that "Business Ethics" is an oxymoron :wink: ... when young and wet behind the ears we tend to be idealistic. Then with accumulated years and experience comes a measure of cynicism as it's an uphill struggle to drain the swamp.
_________________
FWIW, those two DOD tests at and below 2.5V with the infamous 3.44V cell may have resulted in less self-discharge, but still too early to tell. Will post the first 5 days elapsed time (2/15 to 2/20) Saturday afternoon, then after 10 days followed by 15 days (2/15 to 3/2/21).
 
Back
Top