hi guys,
recently i have got a nice milliohm meter and did some measurements right off on my MXUS motors.
the metter is really accurate. i have verified with a high precicse DMM and constant current source.
thats the 3Tx20 motor:
for the 3Tx21 i expected something like 53mOhm or at least lower as the 20strand motor, but WTF?:
neet to check if all strands are properly solderd and especially the delta termination joint.
stock phase wires have 18mOhm (not shortened)
for the 3T motor this would mean 25% of copper losses are in the phase wires. -> not recommended to use it like this.
on 4T it would be about 15%
on 5T about 10%
I also got the new QS 205 V3 with 4T winding (it should be 11,5kV) and measured resistance. it only has 40mOhm incl phase wires. not bad!