well get exited... we sure are! The first frame is coming out of the jig soon. We received the laser cut 4130 frame panels earlier this week and have begun the first production frame.
We plan on testing this frame to it's limits and path-finding the integration of batteries, electronics, and various other things. Once we are satisfied we will begin production of more frames that will be available for sale or custom builds.
Below are some pictures:
laser cut panels
swingarm jig and laser cut panels (sorry blurry)
frame tack welded in jig
frame welding nearing completion
small shop (sorry messy)
We plan on testing this frame to it's limits and path-finding the integration of batteries, electronics, and various other things. Once we are satisfied we will begin production of more frames that will be available for sale or custom builds.
Below are some pictures:
![laser%252520cut%252520frame%252520panels.jpg](/sphere/proxy.php?image=https%3A%2F%2Flh3.googleusercontent.com%2F-PqsKMDp8cZg%2FTwi3jMwC9aI%2FAAAAAAAAALk%2F6F6LwxXtu50%2Fs640%2Flaser%25252520cut%25252520frame%25252520panels.jpg&hash=becc3d22b671f1a36c107fee707b1c95)
laser cut panels
![swingarm%252520jig%252520and%252520laser%252520cut%252520panels.jpg](/sphere/proxy.php?image=https%3A%2F%2Flh6.googleusercontent.com%2F-B--kFpRJ2K8%2FTwi3oznO13I%2FAAAAAAAAAK8%2FVl55pRVXCrk%2Fs640%2Fswingarm%25252520jig%25252520and%25252520laser%25252520cut%25252520panels.jpg&hash=0facf0b2de6016a02fd4cd09f711be6a)
swingarm jig and laser cut panels (sorry blurry)
![tack%252520welded%252520frame%252520in%252520jig.jpg](/sphere/proxy.php?image=https%3A%2F%2Flh6.googleusercontent.com%2F-aw9f8z2Q52M%2FTwi3spTXUDI%2FAAAAAAAAALE%2Fq0rzEscfjZI%2Fs640%2Ftack%25252520welded%25252520frame%25252520in%25252520jig.jpg&hash=24038b6c831a212691cab45245a4adbb)
frame tack welded in jig
![welded%252520frame%252520in%252520jig.jpg](/sphere/proxy.php?image=https%3A%2F%2Flh5.googleusercontent.com%2F-Wzc11sXqZ8c%2FTwi3uL-cqTI%2FAAAAAAAAALM%2F4kWeDKl0dUk%2Fs640%2Fwelded%25252520frame%25252520in%25252520jig.jpg&hash=cbd0742fd12e0b2bb314632091287187)
frame welding nearing completion
![shop%252520panorama.jpg](/sphere/proxy.php?image=https%3A%2F%2Flh3.googleusercontent.com%2F-brhVxHN5eXY%2FTwi3a_sj0OI%2FAAAAAAAAAKs%2FDNs8l3QKbcQ%2Fs640%2Fshop%25252520panorama.jpg&hash=e03e16c986b5f941334cde6d78f44e1d)
small shop (sorry messy)