Experts,
after ending up with 12 badly swollen cells out of my 20 pack of Wina 50Ah LiFePo4 I have learned the hard way that this type of cell must be mechanically contained in order to put a uniform pressure to avoid swelling.
I wonder if I should do the same for winston 40 AH or Sinopoly 40AH LiFePo4?