Sanyo NCR18650BL any good?

nkon is legit. who cares how they group the cells...

my guess is rhe ncr18650bl is similar to the bf... some kind of new chemistry test run.

ncr18650be will still be a better cell for ebike/vehicle.
 
cwah said:
Hello,

I found this:
http://eu.nkon.nl/sony-ncr18650bl.html

Anyone tried or know if these cells are good?
Says on this PDF http://nkon.nl/sk/k/NCR18650BL-specification.pdf
That discharge current should not exceed 7A/cell.

It could be similar to the Sanyo NCR18650BF as it has a similar max discharge rating. http://www.dampfakkus.de/akkutest.php?id=552
http://www.dampfakkus.de/akkuvergleich.php?akku1=507&akku2=552&akku3=490&akku4=353&akku5=523&akku6=258

It could have similar properties as the Samsung 29E where it has a high capacity if the draw is low but will sag and loose its promised capacity at higher draw. (try flicking between 2A and 5A draw on the chart and see the difference in behavior)
 