just finished putting together a rough version of my new and first ebike build!

I'm using a 48V NiCad 5C 8AH Battery with a Clyte 406 and 36-72V 20A pedal first controller with a cycle analyst from Ebikes.ca and was wondering if anyone has a rough idea what I should be setting the LVC to on the Cycle analyst for this particular battery pack. Its resting voltage fresh off the charger is actually 55v or so.
 
what's a good setting for LiFePO4? 55.9V hot off the charger, more typically right around 49.xV after a good ride.
 
Ypedal said:
Toshi said:
what's a good setting for LiFePO4? 55.9V hot off the charger, more typically right around 49.xV after a good ride.

Absolute max low for LiFePo4 = 2.1v under load per cell.
thanks for the reply. does this 2.1V/cell guideline hold true for my 15-cell prismatic LiFePO4 pack, too?

IMG_0026.jpg
 
Thanks Ypedal, Ive been wanting to know about LVC for 48v for a while but never got around to asking. Thanks.
 