braunschweiger
🔋 Established
Could you add for comparison the best in class non-tabless cells for suitable loads (up to 25A) ?I need opinion and suggestions.
Could you add for comparison the best in class non-tabless cells for suitable loads (up to 25A) ?I need opinion and suggestions.
Absolutely. I am working as we speak on Molicel cells. I will keep adding daily new cells to the database. If you have any specific cell you want to request i can add it to the list and put them as priority.Could you add for comparison the best in class non-tabless cells for suitable loads (up to 25A) ?
Molicel p30b would be my reference point for 18650s. thank youAbsolutely. I am working as we speak on Molicel cells. I will keep adding daily new cells to the database. If you have any specific cell you want to request i can add it to the list and put them as priority.
Is the next one on the line.Molicel p30b would be my reference point for 18650s. thank you
Here is you answer at 30A. I do not have to many cells tested at 25A currently.Could you add for comparison the best in class non-tabless cells for suitable loads (up to 25A) ?

The 65P handles 30A better than the 60P that can't even handle 30A at 100% DOD without overtemp ? It thought it would be the opposite
That is correct. The 65P leaved the 60P in the dust. It has even a lower IR. Significant lower.The 65P handles 30A better than the 60P that can't even handle 30A at 100% DOD without overtemp ? It thought it would be the opposite
Do you think the 60P compares to the RH60 ? Btw, have you tested the RH60 already ? I thought the RH60 would be the new budget 6Ah 50S killer at an affordable price. The 65P is still very expensive (however, it seems like it's the perfect cell ever produced yet so worth it)That is correct. The 65P leaved the 60P in the dust. It has even a lower IR. Significant lower.
Basically, most modern all-tab cells designs tend to be very consistent and because of better thermal performance and internal consistency, balancing performance should be better as well.I really like these comparisons.
One question arises though:
How well do these cells balance in a battery pack?
I remember my unpleasant experience with the Samsung 30Q which was quite a remarkable cell otherwise...
Up to 40A test uploaded. I am still testing 45A, 50A, 60a and 100A.Molicel p30b would be my reference point for 18650s. thank you


batteryrealdata.com
60P is definitelly more powerful than RH60, it is close to RS60.Do you think the 60P compares to the RH60 ? Btw, have you tested the RH60 already ? I thought the RH60 would be the new budget 6Ah 50S killer at an affordable price. The 65P is still very expensive (however, it seems like it's the perfect cell ever produced yet so worth it)
However, if I had to choose between thr Linkdata 60P and the RH60, I'd pick the RH60.
Longevity, ease of procurement, extreme consistency, etc.For longevity or something else?
Example: when selecting 21700, 30ACC, all visible models, Voltage over time graph, then this gives a crowded graph with intersecting lines. Identifying the various colors<=>models becomes difficult.I need opinion and suggestions.
![]()
BatteryRealData | Independent Cell Tests vs Manufacturer Datasheets
Independent lithium-ion cell tests that show when cells meet, beat, or fall short of manufacturer datasheet claims.batteryrealdata.com
Shenzhen Genju Technology Co., Ltd. on AlibabaWhich Chinese seller can reliably supply linkdata 65p? I need 120 cells to the UK so don't want to go via US.
Will you be testing GreatPower’s or Amprius’s 60Q recently?Up to 40A test uploaded. I am still testing 45A, 50A, 60a and 100A.
View attachment 389785
View attachment 389786
Compare Battery Test Results | BatteryRealData
Compare real 18650 and 21700 battery discharge tests with a clear, simple workflow for capacity, voltage, temperature, and power.batteryrealdata.com
Cycle life on 60xg was tested on latest version with production data starts like "zg313" ? Because l heard its mass production or on previously with "za"Very recent information. The latest version of the Tenpower 60XG is excellent in terms of discharge characteristics, but unfortunately it suffers from very poor cycle life; based on my actual running test, it appears to last a maximum of 200–300 cycles, regardless of the discharge C-rate. It should be noted that this information is presented in the current datasheet. I'll have the first results for the Amprius 60Q in this discipline within 14 days.