Cam3roon2k41999
1 W
- Joined
- Nov 28, 2021
- Messages
- 59
Hi, I have a BTRpower 60v lipo4 battery( fully charges at 71.4v) and its a 25AH battery,
I've had the battery for about 2 years approximately and I recently noticed that when going on my regular journeys I came back home with less voltage, is it something to worry about or is it normal?
The journeys I take are about 5miles( total) and I used to come home with about 69.5v-70v depending on how I ride etc..
Bit recently taking my time on the journeys I come home with about 64v-66v?
Also I think I'm maintaining the battery correctly as I never leave it without charging it and it's never been left for over 4 days and I always charge the battery after about 10 mins when I come home, also the only thing is the bike is left in a cold environment overnight so could that effect the battery?
Thanks
I've had the battery for about 2 years approximately and I recently noticed that when going on my regular journeys I came back home with less voltage, is it something to worry about or is it normal?
The journeys I take are about 5miles( total) and I used to come home with about 69.5v-70v depending on how I ride etc..
Bit recently taking my time on the journeys I come home with about 64v-66v?
Also I think I'm maintaining the battery correctly as I never leave it without charging it and it's never been left for over 4 days and I always charge the battery after about 10 mins when I come home, also the only thing is the bike is left in a cold environment overnight so could that effect the battery?
Thanks