Yamaha YZ450F

I even have these microballoons:

2h24xNc.jpg


I haven't used this, but something similar a long time ago.
But I thought I would be able to get the fiberglass down there as I had time to go back and forth many times.
I was thinking it would be better in the end to get the strength of the fiberglass holding it together, but ended up with air :rolleyes:
 
Building battery:

fY3sgbg.jpg


It seems I don't have many decent photos, so it seems this will be it for now.
450A fuse might be on the low side, but I have a few of these..
It should be able to take bursts of a lot more it seems:


The voltages were all over the place:

s3KgP1K.jpg


They never were perfectly equal, so it might not be too bad.
I balanced them for a long time, (like 48hours or something) now it looks like this:

FWM1Mz1.jpg


Time will tell :)
 
Hard to see in the picture, but it is very tight to fit the wiring over the cells:

7yYzJtF.jpg


It would probably be possible to get some more room if I built a new top part now when I can see exactly how much room I have over it.

CD0ZVty.jpg


It isn't sealed yet, but still a milestone to have a "finished" battery in place :)
 
Designing some peaces here and there:

1cN2ccy.jpg


Bracket for radiator wings and battery cover.

zFcpC40.jpg


Should slide in here.

Hri0UcD.jpg


I had this skid plate I planned to use with some small modifications.
Well, not much left of it.

ZUq5rv8.jpg


This is how the right side will look.

ZIgtApd.jpg


And the left side will look something like this.

2AqI6Ty.jpg


I will probably bolt this chain guard to the skidplate instead of the motor.
 
I have welded up the front tank cover bracket:

aMbkxSk.jpg


Then I have played a lot with the rear mounting:

SR7QmpW.jpg


I want it to be simple and quick to remove, a problem here is that it doesn't pull down.
I think I will make a similar slide in solution that I have in the front.
It will probably mean that it will be a little tricky to get on and off though :confused:
 
Back