ranjithrajaram8
🧲 New user
Hi all,
I am having the same type of problem in my assembled ebike with 14s5p 21700 battery pack. After installing a smart BMS, i found out the reason. It is Low voltage protection shut off by bms. It shows cell 5 is of low voltage. And by the way i do not have a proper 52v liion charger (awaiting my order to arrive) so will charging the whole pack with a proper charger, fix it or do i need to replace all the cells (5P) at no5 position?
I am having the same type of problem in my assembled ebike with 14s5p 21700 battery pack. After installing a smart BMS, i found out the reason. It is Low voltage protection shut off by bms. It shows cell 5 is of low voltage. And by the way i do not have a proper 52v liion charger (awaiting my order to arrive) so will charging the whole pack with a proper charger, fix it or do i need to replace all the cells (5P) at no5 position?