teslanv
1 MW
Testing a bunch of cells now, and I am coming up with a win for the Samsung 29E. Not the highest capacity or the highest discharge, but the price to overall performance seems to be one of the best.
Anyone think there is a better value cell out there right now?
Looking at building packs in the 16S-20S range and 6P-8P range for the MXUS 3000W Kits we are selling. 40A-60A Discharge rate, typical, so 5A-10A per cell.
Anyone think there is a better value cell out there right now?
Looking at building packs in the 16S-20S range and 6P-8P range for the MXUS 3000W Kits we are selling. 40A-60A Discharge rate, typical, so 5A-10A per cell.