Hello everyone. My name is Aleksei, we are a new startup company called American Electric Solutions LLC, we specialize in refurbishing and destribution of unused Li-Ion battery packs and cells from various suppliers.
This listing is for refurbished and unused 36 Volt 12.8 aH 460 wh Battery pack made with LG MH1 18650 cells.
Condition: Unused. In storage since February 2021 at 50% charge, regularly charged every 2 months. Some battery degradation is expected, but not more than 5%.
All batteries are tested and no battery is below 95% capacity. Any battery that’s below 95% will be exchanged, refunded or partially refunded.
Manufacturer: SCUD LLC. Machine assembled and welded.
Voltage: 36 volt
Capacity: 12.8 Ah 460wh
Cell configuration: 10 Series 4 Parallel
Cell amount: 40
Max recommended discharge rate: 28 amps (or 1000 watts)
Max recommended charge rate: 42 Volts 4 amps ( 3 hours to full charge, 6 hours if charging at 2 amps)
Cycle life: 800-1200 if used gently, 500-700 if used regularly at high discharge rate.
Cell type: LG 18650 MH1 3200mAh Lithium Ion
Weight: 5 lbs
Dimensions:
Length - 8.75 inches
Height - 3.75 inches
Width - 2.75 inches
Nickel strips: Pure 99% nickel, not nickel plated strips, will never rust. Nickel strips are fused for 10 amps, meaning it's thinner in certain parts and will burn off and disconnect the cell in case of over-discharge or over-charge, allowing to save the rest of the pack and replace the cell, instead of the whole battery. Tesla uses the same technology.
Cell holders: Hardened Aero-Grade plastic cell holders with 4 screw holes to hold both parts together and 5 mounting threaded holes for m5 screws or rods. Honeycomb Style.
(Shown in attached pictures)
Connectors: xt60 (bms is locked, read full description)
Isolation: Lithium Ion grade, fiberglass insulating paper with very strong adhesive.
Battery management system: BMS is locked by a chip that requires a certain CAN-BUS communication protocol. At this time it is unknown how to unlock them; we are working on it.
A secondary BMS can be soldered right on top of the existing one, they won’t interfere with each other, the native bms will just act as an additional cell balancer. One non-native bms can be installed on several battery packs to save money and time. They can all be connected in parallel under one bms.
Doesn’t come with a charger.
Shipping via USPS. $16 for a USPS medium flat rate box, can fit up to 5 batteries.
We provide a 45 day warranty on each battery that covers manufacturer defects or unexpected changes in capacity or voltage that’s unrelated to buyers actions like physical damage, extreme discharge rates or temperature-related damage.
Please read general instructions on how to use lithium ion batteries to avoid defects and failures.
If you have any questions about the battery or shipping quotes, pm me or email me at americanelectricsolutions@gmail.com
In the near future all purchases can be made through our website, for now we accept paypal.![1.png 1.png](https://endless-sphere.com/sphere/data/attachments/186/186657-8062cc932abd935bb732c7eabb3ba17e.jpg)
![2.png 2.png](https://endless-sphere.com/sphere/data/attachments/186/186658-a50bf52ff4f595887d8c9dfe8cacafc3.jpg)
![3.png 3.png](https://endless-sphere.com/sphere/data/attachments/186/186659-99b47d76f0f5e05e4395c7b304787247.jpg)
![4.png 4.png](https://endless-sphere.com/sphere/data/attachments/186/186660-e16610f931d36ed85c4a84bf3ac48b63.jpg)
![5.png 5.png](https://endless-sphere.com/sphere/data/attachments/186/186661-d82d06b5ee0fadeb952b0a79be6ee64c.jpg)
![6.png 6.png](https://endless-sphere.com/sphere/data/attachments/186/186662-330b01be3078aa732bec9c0933fec47a.jpg)
![7.png 7.png](https://endless-sphere.com/sphere/data/attachments/186/186663-5c03ce7fa977e816cd3f9a75a4b58ce0.jpg)
![8.png 8.png](https://endless-sphere.com/sphere/data/attachments/186/186664-1e62a3d51d1c1f92765f6526f67523ef.jpg)
![9.png 9.png](https://endless-sphere.com/sphere/data/attachments/186/186665-0ce6f4750f53df6968b73d1c5c142940.jpg)
![10.png 10.png](https://endless-sphere.com/sphere/data/attachments/186/186666-6dc220bc5b30eba817629c28acf8f56b.jpg)
![11.png 11.png](https://endless-sphere.com/sphere/data/attachments/186/186667-cc4b64725323aa9882b1ed6354855edc.jpg)
![12.png 12.png](https://endless-sphere.com/sphere/data/attachments/186/186668-ab29d662c7af225e81662b2d67be177d.jpg)
![13.png 13.png](https://endless-sphere.com/sphere/data/attachments/186/186669-b9b2c448c658ac5e535fb4767e278a6c.jpg)
![14.png 14.png](https://endless-sphere.com/sphere/data/attachments/186/186670-2d4f254b13185f3a023f8c435b4756ae.jpg)
![15.png 15.png](https://endless-sphere.com/sphere/data/attachments/186/186671-f23111e880a18530c9361c29425a7850.jpg)
This listing is for refurbished and unused 36 Volt 12.8 aH 460 wh Battery pack made with LG MH1 18650 cells.
Condition: Unused. In storage since February 2021 at 50% charge, regularly charged every 2 months. Some battery degradation is expected, but not more than 5%.
All batteries are tested and no battery is below 95% capacity. Any battery that’s below 95% will be exchanged, refunded or partially refunded.
Manufacturer: SCUD LLC. Machine assembled and welded.
Voltage: 36 volt
Capacity: 12.8 Ah 460wh
Cell configuration: 10 Series 4 Parallel
Cell amount: 40
Max recommended discharge rate: 28 amps (or 1000 watts)
Max recommended charge rate: 42 Volts 4 amps ( 3 hours to full charge, 6 hours if charging at 2 amps)
Cycle life: 800-1200 if used gently, 500-700 if used regularly at high discharge rate.
Cell type: LG 18650 MH1 3200mAh Lithium Ion
Weight: 5 lbs
Dimensions:
Length - 8.75 inches
Height - 3.75 inches
Width - 2.75 inches
Nickel strips: Pure 99% nickel, not nickel plated strips, will never rust. Nickel strips are fused for 10 amps, meaning it's thinner in certain parts and will burn off and disconnect the cell in case of over-discharge or over-charge, allowing to save the rest of the pack and replace the cell, instead of the whole battery. Tesla uses the same technology.
Cell holders: Hardened Aero-Grade plastic cell holders with 4 screw holes to hold both parts together and 5 mounting threaded holes for m5 screws or rods. Honeycomb Style.
(Shown in attached pictures)
Connectors: xt60 (bms is locked, read full description)
Isolation: Lithium Ion grade, fiberglass insulating paper with very strong adhesive.
Battery management system: BMS is locked by a chip that requires a certain CAN-BUS communication protocol. At this time it is unknown how to unlock them; we are working on it.
A secondary BMS can be soldered right on top of the existing one, they won’t interfere with each other, the native bms will just act as an additional cell balancer. One non-native bms can be installed on several battery packs to save money and time. They can all be connected in parallel under one bms.
Doesn’t come with a charger.
Shipping via USPS. $16 for a USPS medium flat rate box, can fit up to 5 batteries.
We provide a 45 day warranty on each battery that covers manufacturer defects or unexpected changes in capacity or voltage that’s unrelated to buyers actions like physical damage, extreme discharge rates or temperature-related damage.
Please read general instructions on how to use lithium ion batteries to avoid defects and failures.
If you have any questions about the battery or shipping quotes, pm me or email me at americanelectricsolutions@gmail.com
In the near future all purchases can be made through our website, for now we accept paypal.
![1.png 1.png](https://endless-sphere.com/sphere/data/attachments/186/186657-8062cc932abd935bb732c7eabb3ba17e.jpg)
![2.png 2.png](https://endless-sphere.com/sphere/data/attachments/186/186658-a50bf52ff4f595887d8c9dfe8cacafc3.jpg)
![3.png 3.png](https://endless-sphere.com/sphere/data/attachments/186/186659-99b47d76f0f5e05e4395c7b304787247.jpg)
![4.png 4.png](https://endless-sphere.com/sphere/data/attachments/186/186660-e16610f931d36ed85c4a84bf3ac48b63.jpg)
![5.png 5.png](https://endless-sphere.com/sphere/data/attachments/186/186661-d82d06b5ee0fadeb952b0a79be6ee64c.jpg)
![6.png 6.png](https://endless-sphere.com/sphere/data/attachments/186/186662-330b01be3078aa732bec9c0933fec47a.jpg)
![7.png 7.png](https://endless-sphere.com/sphere/data/attachments/186/186663-5c03ce7fa977e816cd3f9a75a4b58ce0.jpg)
![8.png 8.png](https://endless-sphere.com/sphere/data/attachments/186/186664-1e62a3d51d1c1f92765f6526f67523ef.jpg)
![9.png 9.png](https://endless-sphere.com/sphere/data/attachments/186/186665-0ce6f4750f53df6968b73d1c5c142940.jpg)
![10.png 10.png](https://endless-sphere.com/sphere/data/attachments/186/186666-6dc220bc5b30eba817629c28acf8f56b.jpg)
![11.png 11.png](https://endless-sphere.com/sphere/data/attachments/186/186667-cc4b64725323aa9882b1ed6354855edc.jpg)
![12.png 12.png](https://endless-sphere.com/sphere/data/attachments/186/186668-ab29d662c7af225e81662b2d67be177d.jpg)
![13.png 13.png](https://endless-sphere.com/sphere/data/attachments/186/186669-b9b2c448c658ac5e535fb4767e278a6c.jpg)
![14.png 14.png](https://endless-sphere.com/sphere/data/attachments/186/186670-2d4f254b13185f3a023f8c435b4756ae.jpg)
![15.png 15.png](https://endless-sphere.com/sphere/data/attachments/186/186671-f23111e880a18530c9361c29425a7850.jpg)