First test run today, great success
On stock 50 amps battery i hit 80 km/h pretty quick. Now to turn it up to 150 .
Also, I am wondering if I could have burnt out the current measuring part of my CA. Basically my controller should have a shunt value between .6 and .7 mohm. Setting it to these or indeed in the middle gives me nothing on the CA. Anyone know if/how I can check the current sensing hardware in the CA?