silicium said:I tested an LG pack (4P 10S) today:
Discharge 15A constant (about 500W)
The battery returned 10.9 Ah (stop at 2.8V per cell)
At the end, the battery was at 60 ° C ...
I think that we must not exceed 15A continuous discharge for 4P
This battery is excellent for the price !!
ridethelightning said:thanks for that.
so 15A from a 4p pack..
so 3.75a/cell
so if in 10p thats 37.5A
i was wondering about this, good to know what the limits are.
The Mighty Volt said:In fairness, 37.5A from 10p is sh!t.
No. You probably confuse it with Sony US18650VTC5 2500mAh, which may sustain 25A with little cooling.The Mighty Volt said:I agree, but I thought these LG cells were 10c capable, 25A constant...no....![]()
![]()
jimwebo said:10A 4C (In short peak consumption)
Do you understand the concept C. ?
The Mighty Volt said:jimwebo said:10A 4C (In short peak consumption)
Do you understand the concept C. ?
Yes, clearly.
As pointed out above, I was considering a different cell.
jimwebo said:Ok , so the next time before calling sh t. to a product, should be clearer that product is ....
Best regards.
It depends what lgs you are mentioning. But yes, PF is way better then MG1 considering IRridethelightning said:sounds like you expect a lot better performance from the pf than we get from the LGs....
Ch00paKabrA said:Just received my 80 cells for my brother's ebike build. Thank you. I wasn't expecting them for a few weeks and they are here already.