LI-ghtcycle
10 MW
MitchJi said:Hi,
LI-ghtcycle said:I have one of these chargers, and I have looked over this post, but I still can't see why I am having such long charging times when balancing.
I haven't built custom balance plugs yet, so I have just been using the two ports to charge 2 4S batteries at a time, but this is the crazy part!
Ever since I changed the TVC function to charge up to just approximately 4.18 (would have it at 4.15, but that is low as I can see to adjust it so far, just using the charger's menu, haven't been able to use it with my PC yet), it wants to take like 5 years to balance!!
rscamp said:Hmmm. I've had inconsistent readings from balancers before and I eventually traced them to bad connections. The main culprit in my case was high-resistance crimped connections in the connectors for battery balance leads. In my case, the problem occurred after months of use. You could try different balance cables if possible and/or stressing the connections in one way or another and look for changes in the parallel group voltages. If this does something, you are probably on the right track and can replace the connections or try soldering or whatever...
That would explain the inconsistent readings but I don't see how it explains why reducing the voltage increased the charge times.LI-ghtcycle said:Thanks for the idea!![]()
I will try the new balance plugs that came with the Hyperion, this is a good point, I never thought of this!
I have been using the old balance plugs from my last charger (might be a bit warn from use, and lower quality) that would explain the inconsistent readings that have always been on the second set of balance plugs regardless of what battery was being charged! 8)
Well, upon further inspection, I have not found fault with the balance plugs, I still have the "ghost" readings for #8 cell, always higher than the rest, but it does seem to balance things, if I switch things around, everything will be with in .02 V of each other, I guess that is ok. I'm going to call the Hobby Shop and see if they can contact Hyperion and give me some more information.
I know it doesn't make any sense, but after putting the TVC back to factory, it balances much faster?! Doesn't make sense, but it is charging at normal speed now.
One nice thing, maybe this is normal, but even when I have things set at 100% capacity, and factory setting for voltage (4.2V) it seems to get everything to 4.177 - 4.182 and calls it good.