I have a Large Giant DH Team and have a few questions about my build.
This is my bike.

Plan:
Motor: Hubzilla v2 laced into 26inch wheel - Arrived
Controller: Zombies new EB324 board 24FET 150v(135v safe max) 150 amp controller. - Arrived
Zombies throttle tamer - Arrived
Batteries: 8x zippy 6s 8000 mAh (24s 2p). That gives me 88.8 volts and 16 ah. - waiting for stock to come in- ended up getting Turnigy instead.
Charger: iCharger 206B 350W, Powered by a 24V DC 14.6A 350W Regulated Switching Power Supply.
Tires: Maxxis hookworms.
Kiwi’s drop outs - Arrived
For connecting everything up I would love to do something similar to what Tench did.
http://endless-sphere.com/forums/viewtopic.php?f=2&t=39489

Questions:
• I had originally wanted to use Anderson powerpoles and found out that they melt under high power. Will the 75 amp powerpoles also melt under 100volt 100 amp
usage?
• What are the best connectors to use? Polymax 5.5 Gold Connectors? http://www.hobbyking.com/hobbyking/store/uh_viewitem.asp?idproduct=39465
• I was also planning on using 8 AWG wire but I just realized that the wire coming out of the hubzilla V2 is 12 AWG. Does that mean that I will need to rewire the motor's phase wires to keep the insulation from melting off?
This is my bike.

Plan:
Motor: Hubzilla v2 laced into 26inch wheel - Arrived
Controller: Zombies new EB324 board 24FET 150v(135v safe max) 150 amp controller. - Arrived
Zombies throttle tamer - Arrived
Batteries: 8x zippy 6s 8000 mAh (24s 2p). That gives me 88.8 volts and 16 ah. - waiting for stock to come in- ended up getting Turnigy instead.
Charger: iCharger 206B 350W, Powered by a 24V DC 14.6A 350W Regulated Switching Power Supply.
Tires: Maxxis hookworms.
Kiwi’s drop outs - Arrived
For connecting everything up I would love to do something similar to what Tench did.
http://endless-sphere.com/forums/viewtopic.php?f=2&t=39489

Questions:
• I had originally wanted to use Anderson powerpoles and found out that they melt under high power. Will the 75 amp powerpoles also melt under 100volt 100 amp
usage?
• What are the best connectors to use? Polymax 5.5 Gold Connectors? http://www.hobbyking.com/hobbyking/store/uh_viewitem.asp?idproduct=39465
• I was also planning on using 8 AWG wire but I just realized that the wire coming out of the hubzilla V2 is 12 AWG. Does that mean that I will need to rewire the motor's phase wires to keep the insulation from melting off?