I'm all for anything that makes it easier to swap cells, though the trick is in the details. Low voltage, high amp contact connections can easily become high resistance. And we know what happens then.
I think there is a huge market for a power back-up pack for a home, in the 48V-52V range. When everything is going well, we might use "X" amount of kilowatts of energy each month, but I live in tornado country, and it's not unheard of for a wind-storm to knock out power for days, if not weeks.
In that situation, the average person will suddenly re-prioritize their power needs. If someone needs to refrigerate their insulin, then a chest fridge can be a low power device to act as a refrigerator with the temp adjusted to the proper range, and air conditioning can be secondary. Such a person might find themselves using 1/10th the amount of energy they normally would use, but it is the most vital tenth.
I have recently moved, and one of the new purchases was a large chest freezer. Since cold sinks, having the opening on top means that frozen foods can stay frozen for a VERY long time after the power goes out. Even after the frozen goods start to thaw, they are still cold enough to remain unspoiled for an extended time.
A DIY battery pack using pressure contacts is a fantastic home back-up. There is a reduced risk of contact corrosion, and there is no heating-cooling cycles (like a garage) and there is no vibration of sudden pothole shocks.
I want endless-sphere to be the hub for this type of information. If this design works well for Barncat's ebike, sweet. But even if it has enough issues that he upgrades one part of it, the pics and the discussion are saved here for thousands of readers, who will come here because of a google search on this subject.
Great idea! Can you tell us how you built the battery holders? Are they charged by solar or the grid?speaking of home powerwalls, here's mine - 13S/160P, approx 23kWh, double-sided, all recycled 18650-ies, not welded but in batt.holders for ease of exchange.
How are you monitoring the cells? What kind of BMS?i bought d batt.holders, see pic. i am charging 99% by solar, but still have option to connect to grid for back-up.
I don't believe a BMS is necessary. I'M the BMS. There is instant DMM access to each parallel cell group down one side to check voltage and at the ends for pack V.
Hi Barncat, Can you post a photo of the 3/4" braided copper strap installed, making contact with the 5 cells?I used .025" copper strips to parallel the cells on the original 18650 pack, but they proved to have inconsistent contact for larger 21700 cells, hence the clever use of the 3/4" braided copper strap, which conforms perfectly to the cell ends, carries a lot of current, and also dampens vibration. You don't want any loose whiskers on that material, so the ends are fluxed and tinned and then cut to exact length to span 5 cells.