I have worked a lot on the bike, there just isn't that much result to show..
I fixed the finish on the upper part of the battery box.
It isn't perfect, because I took too much with a 240 paper.
I didn't have anything between 240 and 1000..
I can take more with 1000, but I don't want the gelcoat to be thinner than necessary.
I finished off with 1500 and then 3000.
A before picture.
The inside is pretty much done, some tiding up the wiring and sealing stuff left to do.
Making the mounts..
It is a lot easier when you can just get in position and spot weld with the mig/mag.
I have to get things in position and take out the battery, tig it in position and check and adjust.

I fixed the finish on the upper part of the battery box.
It isn't perfect, because I took too much with a 240 paper.
I didn't have anything between 240 and 1000..
I can take more with 1000, but I don't want the gelcoat to be thinner than necessary.
I finished off with 1500 and then 3000.

A before picture.

The inside is pretty much done, some tiding up the wiring and sealing stuff left to do.

Making the mounts..
It is a lot easier when you can just get in position and spot weld with the mig/mag.
I have to get things in position and take out the battery, tig it in position and check and adjust.