Thanks, it was just the top one on the first picture I had to add material on.
Otherwise there would have been a thin section, the 3 cells to the left are all parallel. So especially where they meet the 4:th cell would be a weak spot.

I cant really shake off that maybe I should go 28s11p instead of 30s10p like this is..
It is nice to be able to use the same chargers as the other bike, but less controller options :unsure:
 
Alright, so now it is pretty much no turning back as I ordered the busbars.

I asked if they could include a few extra of the small square pieces that welds to the cells, so I could do some testwelds on old cells.
But they couldent understand what I wanted, after some back and forth they asked me to send a picture.

Jx8ogPO.jpg


I sent this, and got the reply "those are included" and they sent a picture of a battery pack with welded busbars.
I gave up after that :rolleyes:
 
The copper plates arrived a few days ago:

4JjQey4.jpg


About 2kg for one battey :confused:
Maybe I should have asked for 0,5mm thick, they suggested 1mm and I didnt disagree.
As I dont have any weak spots really, 0,5mm should be more than enough I think.
My weakest is 3 parallel cells have to share a 30mm wide "passage". So now it is 30mm2, in 0,5mm it would still be 15mm2.
 
Alright, so now it is pretty much no turning back as I ordered the busbars.

I asked if they could include a few extra of the small square pieces that welds to the cells, so I could do some testwelds on old cells.
But they couldent understand what I wanted, after some back and forth they asked me to send a picture.

Jx8ogPO.jpg


I sent this, and got the reply "those are included" and they sent a picture of a battery pack with welded busbars.
I gave up after that :rolleyes:
Can you post your listing of the product you ordered? Because it probably defines the thickness of the nickel they use. And you could just order the same thickness nickel, in separate strip form, for your test welds to find your settings.
About 2kg for one battey :confused:
Maybe I should have asked for 0,5mm thick, they suggested 1mm and I didnt disagree.
As I dont have any weak spots really, 0,5mm should be more than enough I think.
My weakest is 3 parallel cells have to share a 30mm wide "passage". So now it is 30mm2, in 0,5mm it would still be 15mm2.
Don't feel bad, I just put 3.6kg of copper onto my battery!

Anyway, You'll have much less resistance with the 1mm copper, that will be nice
 
No need to worry about 1 or 2 kg , I have installed 120mm² copper bus bars 3mmx40mm.
Only a little bit oversized. 😉 My battery can do 800A continous.
The other option I had was 0.8x40mm which was mechanicaly to weak for me.
Screenshot_20240418_233011_Samsung Internet.jpg
 
Last edited:
Can you post your listing of the product you ordered? Because it probably defines the thickness of the nickel they use. And you could just order the same thickness nickel, in separate strip form, for your test welds to find your settings.
Problem is that it is not nickel, I think it is nickel plated copper. And there is a slit in the middle.
What's your anticipated peak battery current?
10p of molicell p45b, so I suppose 450A, maybe I can go a little higer for my short 2sec bursts? 500 or so.
 
Suddenly without any warning these turned up:

jgvY3XE.jpg


The tracking number I got still hasnt moved..
I have been chasing info about how to decipher the numbers, eventually I found this:

4nUW7Re.jpg


I suppose that means they should be manufactured 18:th January 2024?
All the cells I have looked at has the exact same numbers, not sure if that is a good or bad thing?

bSlMz3o.jpg


kRmAMs8.jpg


Under the wrap.
So, I think there are 3 possibilities here:
1: everything is fine, they are newly manufactured molicel P45B.
2: They are factory rejects, like B, C grade or something.
3: They are fake.

I think 2 are less likely as they seem to all be the same batch as they have the same numbers?
If they dont discard whole batches when they discover a problem, that might actually be kind of likely :unsure:
 
Testing batteries..

IpqaOm7.jpg


5THn7dn.jpg


All the ones I have tried so far has ended just under 4000mah at 1A discharge.
But the test ends when one cell reach 2,5V, some cells can then be at about 2,8V.
I have seen close to 3V in one test. dont really know how much that means in mah, but I am doing a small test of the difference between the best and worst cells on the side.
I am testing 10 cells at a time, this should take about a month like this I think. I dont even want to think about testing one at a time :oop:
According to the data sheet I should be getting at least 4300mah

https://www.molicel.com/wp-content/...roduct-Data-Sheet-of-INR-21700-P45B-80109.pdf
 
According to the data sheet I should be getting at least 4300mah
That's disappointing... you purchased these new?

Especially since you're testing at 1A discharge, you should be getting the rated 4300-4500mah at such a low discharge rate.
 
Yes, they are new.
I better make a correction, all the tests have ended at just under 4000mah.
Meaning the lowest capacity cell (of 10) in each test ended there, the others would test higher.
But still, yes I think they should end over 4300mah.
I think I should get some other cells to test for reference.
 
Good luck getting to the bottom of the capacity results with the cells, hopefully it is just a calibration/reference issue with your equipment!
 
That's close enough in my opinion. I'd be more focused at the internal resistance, it says a lot more about a cell health than its capacity usually.
Did you make sure the cells were fully charged before the discharge test (I think you probably did, but better check the obvious things first). Also make sure you have excellent contact between the cell and the device that measures discharge. If you are lucky enough to have a thermal imaging camera it can help you a lot to find if there's something wrong in your setup.
 
I do a charge (to 4,2V) and discharge cycle in each test, so I think that part should be ok.
I havent made any changes to hold times or anything like that, it is definitely possible that it is just a settings problem.
Or for that matter a calibation issue.
I think at these low currents my cell holders should be enogh, at higher currents these would surely be a problem.

I realize I dont have any picture of my test rig, I will try to get that in the evening.

I will get to internal resistance soon. My charger shows a value, it has been between 20-30mOhm, but I dont trust that to be accurate. I dont have any real tester for it, I will try to just mesure voltage drop and current.
 
Sorry, it took a little longer. I have been very busy in the evenings.
This is what the test rig looks like:

n8BbKFI.jpg


An icharger 4010 duo and simple cellholders. I noticed I am able to log both channels at the same time, but there was missing pins in one cellholder. So I was only able to set up one 10s channel, the other one is just 8s.

I have also ran a test of two of the best performing, and two of the worst performing cells in this opus charger:

wvbe43p.jpg


They are not up there in capacity in that test either, but it looks like they are not to far apart from each other at least.

I have started a little with ir tests, but I dont have a proper test rig for that.
I tried this:

3S3mLEf.jpg


I think I need to make something better, but this is one measurement:

wcrFBY2.jpg


This is 13mOhm, but I have also measured 17mOhm:s on the same cell, and this is at 20'C and 3,7V.
 
Okay, my battery holder is done.

gUQBS8R.jpg


The parts used, alu screws I had that felt ok for the job.
2 small brass nails that I soldered small wires to the edge on.
3d printed holder and sleeves for the nails.
2 ballpoint pen springs.
Another spring for one of the screws.

ubhvWHb.jpg


A little machining of the screws: a 2,5mm hole right through for the wires and a 4mm seat for the spring.

LdVZzUV.jpg


And finished :)
Now I just have to determine how I should test..

(Yea, Idont really know what I was thinking when I made it that long with that long spring..)
 
I got a delivery a while ago:

xoQJe3I.jpg


I was in a hurry to order, as I expected it to take a long time to get it.
But it actually showed up in about a month, as it was supposed to.

9W8OjNN.jpg


All black should mean v4 as far as I know, but pin 12 is dead short to ground :(
On the 700/1000 v4 models it should be a "mode" input, but not cl1400 it seems.

It should be possible to use the sin/cos inputs instead according to Hackey, but it seems impossible to get him to say how..
 